The application of welding robots has brought very good income to the welding field, because welding robots are convenient to operate and their work efficiency is 3 times that of normal employees. Welding robots can well protect the safety of welding workers. Welding robots have completely replaced manual labor. The robot welding uses argon-rich mixed gas shielded welding. The welding defects that appear during the welding process generally include welding deviation, undercut, and pores. The specific analysis is as follows:
(1) The occurrence of welding deviation may be caused by incorrect welding position or problems when searching for the welding gun. At this time, it is necessary to consider whether the TCP (the position of the center point of the welding gun) is accurate and adjust it. If this happens frequently, check the zero position of each axis of the robot, and re-calibrate to correct it.
(2) The occurrence of undercut may be due to improper selection of welding parameters, incorrect welding torch angle or welding torch position. You can appropriately adjust the power to change the welding parameters, adjust the torch posture and the relative position of the welding torch and the workpiece.
(3) The porosity may be due to poor gas protection, the primer of the workpiece is too thick, or the protective gas is not dry enough, and it can be dealt with by corresponding adjustments.
(4) Excessive spattering may be due to improper selection of welding parameters, gas composition reasons, or too long outer elongation of the welding wire. You can adjust the power to change the welding parameters, adjust the gas proportioner to adjust the mixed gas ratio, and adjust the welding gun and The relative position of the workpiece.
(5) An arc crater is formed at the end of the weld after cooling, and the submerged arc crater function can be added to the work step during programming to fill it.